CuSn12 – 7013/2
CC483KG-SnBz12 DIN 1705
CuSn12Ni2
CC484KG-SnBz12Ni2 DIN 1705
|
Material |
Tensile Strength |
Yield Strength |
Elongation A% |
Brinell Hardness |
|
Cusn12 |
27÷32 |
15÷17 |
5÷10 |
90÷100 |
|
Material |
|
Sn% |
Zn% |
Pb% |
Fe% |
Ni% |
Ai% |
P% |
Si% |
Mn% |
Sb% |
As% |
Cu% |
|
CuSn12 |
Min% |
11.00 |
0 |
0 |
0 |
0 |
0 |
|
0 |
0 |
0 |
|
85 |
|
Max% |
13.00 |
0.5 |
1 |
0.2 |
0.7 |
0.1 |
|
0.02 |
0.02 |
0.02 |
|
89 |
|
|
CuSn12Ni2 |
Min% |
11.00 |
0 |
0 |
0 |
1.5 |
0 |
|
0 |
0 |
0 |
|
84.5 |
|
Max% |
13.00 |
0.5 |
0.3 |
0.2 |
2.5 |
0.1 |
0.4 |
0.01 |
0.2 |
0.1 |
|
87.5 |
N.B.: The values shown in the table are indicative.